Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88
88
ASTM D785
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Ultimate 100 MPa
14500 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
ASTM D790
Compressive Yield Strength 103 MPa
14900 psi
ASTM D695
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
379 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: