Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer APA - Advanced Polymer Alloys
Trade Name Alcryn®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high productivity on thermoplastic processing equipment.Applications:Window and door weatherstripping (and other complex profile extrusions)Soft handles and gripsMolded seals and gasketsInjection-molded and co-injection molded partsBlow-molded partsTubing and hoseWire and cable jacketsCoated fabrics and sheet goodsInformation provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D471; ISO 2781
Viscosity 870000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
870000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
After 7 days at 257°F (125°C); ASTM D573; ISO 188
78
78
ASTM D2240; ISO 48
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D412; ISO 37
11.6 MPa
1680 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Elongation at Break 350 %
350 %
After 7 days at 257°F (125°C); ASTM D573; ISO 188
360 %
360 %
ASTM D412; ISO 37
100% Modulus 0.00510 GPa
0.740 ksi
ASTM D412; ISO 37
0.00869 GPa
1.26 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Graves Tear Strength 54.3 kN/m

@Temperature 23.9 °C
310 pli

@Temperature 75.0 °F
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 9.0
9.0
Cs-17 Wheel, 1000 g Load; ASTM D3389
Compression Set 25 %
25 %
After 22 Hr at 75°F (24°C); ASTM D395; ISO 815
74 %

@Temperature 100 °C
74 %

@Temperature 212 °F
22 hrs.; ASTM D395; ISO 815
Tensile Set 12 %
12 %
ASTM D412
Torsional Stiffness 4.134 MPa
599.6 psi
At 75°F (24°C); ASTM D1043
68.9 MPa
9990 psi
At -4°F (-20°C); ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746; ISO 812
Clash Berg Stiffness Temperature 3.89 °C
39.0 °F
At 10,000 psi (69 Mpa); ASTM D1043
Processing Properties Metric English Comments
Processing Temperature 166 °C
330 °F
Descriptive Properties Value Comments
Fluid Resistance - Volume Change, % (ASTM D471) -10
After 7 Days in ASTM Oil No.1 at 212°F (100°C)
11
After 7 Days in Water at 212°F (100°C)
26
After 7 Days in IRM 903 Oil No.3 at 212°F (100°C)
26
After 7 Days in ASTM Ref. Fuel No. B at 75°F (24°C)
Users viewing this material also viewed the following: