Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | ASTM D638 |
Multibase Multi-Flex® TPE G 7455 X Multi-Flex® G 7455 X is based on the Kraton G 78455 X formulation. It has low specific gravity as well as having a UL 94 rating of V-0. Ash is 5.2%. Multi-Flex TPE contains Kraton™ G.Data provi.. |
|||
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber
(discontinued **) A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr.. |
|||
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | ASTM D638 |
Colorite Polymers 6533 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | ASTM D412-75 |
3M SJ-1FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | ASTM D412-75 |
3M SJ-2FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | ASTM D412-75 |
3M SJ-3FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Tensile Strength, Ultimate | 11.6 MPa | 1680 psi | ASTM D412-75 |
3M SJ-4FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |