Alloy Wire International RW 41 Hot Cutting Wire - Ultra High Strength

Category Metal
Manufacturer Alloy Wire International
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alloy Wire International RW 41 Hot Cutting Wire - Ultra High Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and other materials. May be used on oscillating cutting frames in continuous service.Information provided by Alloywire International.
Physical Properties Metric English Comments
Density 8.25 g/cc
0.298 lb/in³
Thermal Properties Metric English Comments
CTE, linear 13.6 µm/m-°C

@Temperature 20.0 - 100 °C
7.56 µin/in-°F

@Temperature 68.0 - 212 °F
Melting Point 1345 °C
2453 °F
Maximum Service Temperature, Air 300 °C
572 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000131 ohm-cm

@Temperature 20.0 °C
0.000131 ohm-cm

@Temperature 68.0 °F