Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.25 g/cc | 0.298 lb/in³ | Sintered (HIP) |
Kinetics MIM F1537 (ASTM F1537) HIP and Heat Treat Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | Sintered |
Kinetics MIM F75 (ASTM F75) HIP Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
IBC Advanced Alloys 41C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
IBC Advanced Alloys FA230 Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Indium Corp. Indalloy 105 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Haynes R-41 alloy, 0.635 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Latrobe DuraTechâ„¢ M48 Powder Metal High Speed Steel (ASTM M48) DuraTech M48 super high speed steel is a high-performance high speed steel which exhibits superior hot (red) hardness compared to T15 and M42 high speed steels, and wear resistance comparable to tha.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Special Metals UDIMET® alloy R41 Ni-Cr Alloy UDIMET® alloy R41 (UNS N07041) is a precipitation-hardenable nickel-chromium alloy containing significant amounts of cobalt and molybdenum, along with lesser amounts of aluminum and titanium. Al.. |
|||
Density | 8.24 g/cc | 0.298 lb/in³ | |
Wall Colmonoy COLMONOY® 52 SA - Hard Nickel-Chromium-Boron Alloy Containing Chromium Carbides Description and Application: Similar to Colmonoy No. 62 SA, but has increased ductility with almost the same abrasion and corrosion resistance. Finished by grinding.Method of Application: Sprayweld.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Cadi 3 MOLD-MOR™ The hardest and highest strength copper alloy, Beryllium copper is specified when the mechanical strength is the limiting design feature for a copper alloy.Forms: RodBarPlateInformation provided by .. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
California Fine Wire Alloy 52 Nickel Iron Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
California Fine Wire Stablohm 675 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Alloy Wire International RW 41 Hot Cutting Wire - Ultra High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and other materials. May be used on oscillating cutting frames in continuous service.Information .. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
ATI Allegheny Ludlum Moly Permalloy Electrical Alloy An alloy with exceptionally high magnetic permeability, very low coercive force, very low core losses, and low reminance by magnetic field annealing. The alloy finds application in magnetic shieldi.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |
|||
Density | 8.24 g/cc | 0.298 lb/in³ | |
ATI Allvac® M-252 Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal Applications: Turbine blades, fasteners, and high temperature bolting.Data provided by Allvac. |
|||
Density | 8.24 g/cc | 0.298 lb/in³ | |
ATI Allvac® Nickelvac® W-722 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Ring components in jet engines. |
|||
Density | 8.24 g/cc | 0.298 lb/in³ | |
ATI Allvac® Nickelvac® X- 751 UNS N07751 Nickel Superalloy Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines.Property values are for samples in the metallurgical condition: 1800°F age.Information provided by Allv.. |
|||
Density | 8.24 g/cc | 0.298 lb/in³ | |
Wall Colmonoy COLMONOY® 5 - Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides Description: Contains wear-resistant chromium borides and carbides. Has greater ductility, better impact resistance and workability than Colmonoy No. 6 Finished with carbide tools and grinding.App.. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include .. |
|||
Density | 8.25 g/cc | 0.298 lb/in³ | |
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |