Material Notes:
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can be used in food contact applications with the appropriate stabilizer package
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 2782
Viscosity Measurement 15

@Temperature 180 °C
15

@Temperature 356 °F
Kg/cm<sup>2</sup>; Macklow-Smith extrusion rheometer
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ISO 868
Tensile Strength 7.20 MPa
1040 psi
ISO 37
Elongation at Break 455 %
455 %
ISO 37
100% Modulus 0.00560 GPa
0.812 ksi
ISO 37
Tear Strength 46.0 kN/m
262 pli
ISO 34-B
Compression Set 54 %

@Temperature 70.0 °C,
Time 79200 sec
54 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -60.0 - -50.0 °C
-76.0 - -58.0 °F
Descriptive Properties Value Comments
Bonds with Polypropylene
Chemical Resistance Acetone
Moderate
Acids up to 80%
Good
Alcohol
Good
Alkalis
Good
Brake fluid
Moderate
Chlorinate solvents
Poor
Diesel
Poor
Ethylene glycol
Excellent
Gasoline
Poor
Salt solution
Good
Soda lye
Good
Water, 23°C
Excellent
Water, 95°C
Moderate
Transparency Opaque