Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.812 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00560 GPa
0.812 ksi
ASTM D412
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure..
100% Modulus 0.00560 GPa
0.812 ksi
ASTM D412-80
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (discon
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
100% Modulus 0.00560 GPa
0.812 ksi
TPE-0153 (ASTM D 412)
ExxonMobil Vyram™ 9271-85 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure..
100% Modulus 0.00560 GPa
0.812 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00560 GPa
0.812 ksi
DIN 53504
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
100% Modulus 0.00560 GPa
0.812 ksi
0.025" extruded film; DIN 53504
Huntsman IROGRAN® PS442-202 TPU-Polyester
Introduction: IROGRAN PS440-202 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN PS440-202 is part of the HUNTSMAN ..
100% Modulus 0.00560 GPa
0.812 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00560 GPa
0.812 ksi
Vulcanizate, Press cured, TC95 +3min at 180°C
Dow Nordel® IP 4770P Heat Resistant Peroxide Compound
FormulationNordel® IP 4770P
100% Modulus 0.00560 GPa
0.812 ksi
Vulcanizate, Press cured, TC95 +3min at 180°C
Dow Nordel® IP 4770R Heat Resistant Peroxide Compound
FormulationNordel® IP 4770R
100% Modulus 0.00560 GPa
0.812 ksi
ISO 37
AlphaGary Evoprene™ G 964 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
100% Modulus 0.00560 GPa
0.812 ksi
ISO 37
AlphaGary Evoprene™ GC 640 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..