AlphaGary Garaflex™ G 7765-A5R Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer AlphaGary
Trade Name Garaflex™ G
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garaflex™ G 7765-A5R Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Garaflex™ G is a thermoplastic elastomer intended for wire and cable applications105°C rated TPE for wire and cable applications including welding cables
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
Tensile Strength 17.9 MPa
2600 psi
Elongation at Break 580 %
580 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 °C
-76.0 °F
Oxygen Index 23 %
23 %