AlphaGary Megolon™ S560UV Low Smoke Halogen Free

Category Polymer , Thermoplastic
Manufacturer AlphaGary
Trade Name Megolon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Megolon™ S560UV Low Smoke Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sheathing compound with good mechanical properties in combination with good fire and water resistant properties. Designed for optical cables. Application example includes Telephone Optical
Mechanical Properties Metric English Comments
Tensile Strength 10.5 MPa
1520 psi
Elongation at Break 150 %
150 %
IEC60811-1-1
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 143 °C
290 °F
Temperature Index
Oxygen Index 36 %
36 %