Material Notes:
Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Conditioned; ISO 868
85
85
ISO 868
Tensile Strength at Break 40.0 MPa
5800 psi
Conditioned; ISO R 527
70.0 MPa
10200 psi
ISO R 527
Elongation at Yield 6.0 %
6.0 %
ISO R 527
11 %
11 %
Conditioned; ISO R 527
Modulus of Elasticity 1.50 GPa
218 ksi
Conditioned; ISO 178
3.80 GPa
551 ksi
ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180/1A
6.00 kJ/m²
2.86 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/IeU
NB
NB
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/IeA
0.500 J/cm²
2.38 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C
27.8 µin/in-°F
ASTM E831
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
Conditioned; CEI 60243-1
28.0 kV/mm
711 kV/in
CEI 60243-1
Comparative Tracking Index 600 V
600 V
CEI 60112/Solution A