Material Notes:
CHARACTERISTICS: HIGH CLARITY, HIGH FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING FOR FOOD CONTAINERS, HOUSEWARES, CRATES
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 35 %
35 %
ASTM D638
Flexural Modulus 1.08 GPa
157 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.380 J/cm

@Temperature 23.0 °C
0.712 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 83.0 °C
181 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 180 - 230 °C
356 - 446 °F