Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amco Amalloy® B1044 Polymer Alloy

Category Polymer , Thermoplastic
Manufacturer Amco Plastic Materials
Trade Name Amalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco Amalloy® B1044 Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D1505
Melt Flow 1.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
1.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Flexural Modulus 2.93 GPa
425 ksi
ASTM D790
Impact 170
170
lbs. Instrumented Impact - Max Load
Impact Test 0.904 J
0.667 ft-lb
Instrumented Impact - Energy to Max; Amco Internal Test
Thermal Properties Metric English Comments
Vicat Softening Point 98.3 °C
209 °F
ASTM D648
Optical Properties Metric English Comments
Haze 0.30 %

@Thickness 2.54 mm
0.30 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 91.7 %

@Thickness 2.54 mm
91.7 %

@Thickness 0.100 in
ASTM D1003
Users viewing this material also viewed the following: