Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 30-005W Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hysun™ 383 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Ineos H44N-00 Polypropylene Homopolymer H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Spartech SP-9020 Premium ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES HiFill® TPX-PVDF-03009 C Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerFeatures: Low Shrinkage and Low Smoke EmissionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS 8009 FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 8325 ABS, Sheet Coextrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnumâ„¢ FG960 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
PlastxWorld CEVIAN® E80 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 5140H Compression Molding Polypropylene HomopolymerApplications: Compression Molded Caps and Closure ApplicationsFormolene 5140H DEVELOPMENTAL is a polypropylene homopolymer designed and formulated for compression molded caps and closure .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
CPC - Vycom PROTEC® Homopolymer Polypropylene Protec HP is a high corrosion resistant polypropylene material which exhibits excellent tensile strength and stiffness at elevated temperatures. Homopolymer polypropylene possesses excellent resista.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP30-1200S Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in/min (50 mm/min); ASTM D-638 |
Bapolene® 4052F Polypropylene, Blown Film Grade Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
Atom Adhesives AA-BOND FS227 Epoxy Adhesive AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, a.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Aaron Industries AVPP HOMO 200-1 Virgin Polypropylene A virgin polypropylene specifically designed for all injection molding applications. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Albis Plastics ASA 02A MR20 , 20% Mineral Filled
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate
(discontinued **) Plasticizer 25%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5390 psi | ASTM D638 |
Aclo Accucomp ABS ABS801V Automotive Approved Grade |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 25% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |