Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.96 GPa | 429 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/10T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | ASTM D638 |
PolyOne Nymax™ 600 A Zip 23 Natural 1 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | ASTM D638 |
PolyOne Nymax™ 600 A Zip 43 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | chs 2 in/min; ASTM D638 |
Network Polymers NPS 80-1800 Crystal Polystyrene Description: Injection Molding Grade, High Melt FlowInformation provided by Network Polymers Inc. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Fiberfil® PP-60/TC/30 Polypropylene Homopolymer, 30% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | ISO 527 |
FKuR Kunststoff Bio-Flex® F 6513 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific) LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D 638 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Total PSC 535 Polystyrene Polystyrene 535 is a high heat crystal polystyrene designed for injection molding, extrusion and blow molding. The material demonstrates excellent strength and good temperature resistance. The varie.. |
|||
Tensile Modulus | 2.96 GPa | 429 ksi | |
Hexcel® HexPly® F593 Epoxy Resin HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
American Polymers API 395 Polystyrene API 395 is one of the highest flowing crystal polystyrenes commercially available. It is produced in pellet form for injection molding and compounding. This material is designed for hard to fill .. |
|||
Tensile Modulus | 2.96 GPa @Temperature 22.8 °C |
430 ksi @Temperature 73.0 °F |
ASTM D638 |
Ensinger TECAPEI® made from Ultem® 1000 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D-638 |
Axiall LR-5009 Rigid PVC, Molding, All Colors Georgia Gulf LR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent process ability,.. |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |
|||
Tensile Modulus | 2.96 GPa | 430 ksi | ASTM D638 |
Amco Amalloy® B1044 Polymer Alloy Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials. |