Features:nucleatedanti-statgood processabilitygood stiffnessApplications:containerscapsclosurestoysFormer A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc

@Temperature 23.0 °C
0.902 g/cc

@Temperature 73.4 °F
ASTM D792
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Elongation at Yield 7.5 %
7.5 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
.05 in/min, 1% Secant; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648