American Elements Yttria stabilized Zirconia

Category Ceramic
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Yttria stabilized Zirconia.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionYttria stabilized Zirconia or Zirconium Oxide Nanopowder or Nanoparticles (YSZ), nanodots or nanocrystals are white high surface area particles available fully stabilized (8 mol%) or partially stabilized ( 3 mol%) or doped with yttria (yttrium oxide). Nanoscale Yttria stabilized Zirconia or Zirconium Oxide is typically 5 - 100 nanometers (nm) with specific surface area (SSA) in the 25 – 50 m 2 /g range. Nano Yttria stabilized Zirconia or Zirconium Oxide Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Yttria stabilized Zirconia or Zirconium Oxide nanocrystals include as in micro-ceramics, in solid oxide fuel cell (SOFC) electrolyte microlayers or films, and in coatings, thermal coatings, plastics, nanowire, nanofiber and textiles and in certain advanced ceramic applications.
Physical Properties Metric English Comments
Particle Size 0.0050 - 0.10 µm
0.0050 - 0.10 µm
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g