American Polymers API 375 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer American Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Polymers API 375 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
API 375 is a general purpose polystyrene produced in pellet form for injection molding. API 375 has excellent strength and clarity as well as fast set-up properties.Applications: Used in the manufacture of containers, housewares, toys and medical applications.Information provided by American Polymers, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min
5.0 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 76
76
ASTM D785
Tensile Strength, Ultimate 44.5 MPa
6450 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 2.85 GPa
413 ksi
ASTM D638
Izod Impact, Notched 0.160 J/cm

@Thickness 3.17 mm
0.300 ft-lb/in

@Thickness 0.125 in
injection molded sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C
195 °F
Annealed; ASTM D648
Vicat Softening Point 102 °C
215 °F
ASTM D1525