Material Notes:
High strength alumina (96%) available pink or white. Available in many shapes and sizes.Information provided by Anderman Ceramics.
Physical Properties Metric English Comments
Density 3.65 g/cc
0.132 lb/in³
Open Porosity 0.00 %
0.00 %
Gas Tight
Mechanical Properties Metric English Comments
Hardness, Mohs 9.0
9.0
Tensile Strength 131 MPa
19000 psi
Flexural Strength 310 MPa
45000 psi
Thermal Properties Metric English Comments
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 23.0 W/m-K

@Temperature 20.0 - 100 °C
160 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Component Elements Properties Metric English Comments
Al2O3 96 %
96 %
B2O3 <= 0.010 %
<= 0.010 %
CaO 0.020 %
0.020 %
Fe2O3 0.010 %
0.010 %
MgO 0.020 %
0.020 %
Na2O 0.14 %
0.14 %
SiO2 3.6 %
3.6 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm

@Temperature 600 °C
1.00e+6 ohm-cm

@Temperature 1110 °F
1.00e+14 ohm-cm

@Temperature 20.0 °C
1.00e+14 ohm-cm

@Temperature 68.0 °F
Dielectric Constant 9.3

@Frequency 1.00e+6 Hz
9.3

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Thermal Shock Resistance Medium
Users viewing this material also viewed the following: