AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets

Category Polymer , Thermoplastic , Polyurethane, TP , Silicone Polyurethane, Ether Based
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc and THF. Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Physical Properties Metric English Comments
Molecular Weight >= 95000 g/mol
>= 95000 g/mol
Mn by GPC using polystyrene stds; TM-005
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 88
78 - 88
TM-025
Tensile Strength at Break 15.0 - 30.0 MPa
2180 - 4350 psi
TM-019G
Tensile Stress 4.00 - 6.00 MPa

@Strain 100 %
580 - 870 psi

@Strain 100 %
TM-019G
5.00 - 8.00 MPa

@Strain 200 %
725 - 1160 psi

@Strain 200 %
TM-019G
7.00 - 11.0 MPa

@Strain 300 %
1020 - 1600 psi

@Strain 300 %
TM-019G
Elongation at Break >= 500 %
>= 500 %
TM-019G
Modulus of Elasticity 0.0100 - 0.0200 GPa
1.45 - 2.90 ksi
TM-019E
Tear Strength 50.0 - 70.0 kN/m
285 - 399 pli
TM-019K
Descriptive Properties Value Comments
Polydispersity 1.6-2.2
TM-005; Mw/Mn by GPC using polystyrene stds