Applied Composites 8050 Polyester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Applied Composites Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8050 Polyester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: Radiant Panel, UL 94-VO, Low Shrink, PigmentableInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 55
55
ASTM D2583
Tensile Strength, Ultimate 96.5 MPa
14000 psi
ASTM D638
Tensile Modulus 13.1 GPa
1900 ksi
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
Secant at 2.5 Deflection; ASTM D790
8.62 GPa
1250 ksi
Secant at 0.5 Deflection; ASTM D790
11.7 GPa
1700 ksi
Tangent; ASTM D790
Compressive Strength 165 MPa
24000 psi
ASTM D695
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.81 J/cm

@Temperature 23.0 °C
9.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C
>= 450 °F
Flexural Load; ASTM D648
Flammability, UL94 V-0
V-0
1/16 in, Equivalent to UL94-V5; UL746
V-0
V-0
1/4 in, Equivalent to UL94-V5; UL746
V-0
V-0
1/8 in, Equivalent to UL94-V5; UL746