Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Applied Composites 8072 Polyester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Applied Composites Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8072 Polyester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industry Application: TransportationProduct Application: AutomotiveDistinct Features: Zero Shrink, Superior Class A Finish, Improved Impact, Accepts Mold CoatingInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.88 g/cc
0.0679 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 35
35
ASTM D2583
Hardness, Rockwell M 102
102
ASTM D785
Tensile Strength, Ultimate 68.9 MPa
10000 psi
ASTM D638
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Flexural Strength 148 MPa
21500 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
Tangent; ASTM D790
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.10
0.10
% Loss 1000 Cycles; FTMS1091
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flexural Load; ASTM D648
Users viewing this material also viewed the following: