Material Notes:
Industry Application: ConstructionProduct Application: Building ProductsDistinct Features: Pigmentable, High Molding Efficiency, Low Thermal ExpansionInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 115
115
ASTM D785
Tensile Strength, Ultimate 48.3 MPa
7000 psi
ASTM D638
Tensile Modulus 10.3 GPa
1500 ksi
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
Tangent; ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.20
0.20
% Loss 1000 Cycles; FTMS1091