Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aquabond Technologies Aquabond™ ABS-85 Water Soluble Adhesive and Bonding Thermoplastic

Category Polymer , Adhesive , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer Aquabond Technologies
Trade Name Aquabond™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aquabond Technologies Aquabond™ ABS-85 Water Soluble Adhesive and Bonding Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding temperatures that can be purchased in either stick or bulk form. All products are virtually insoluble in cold or cool water, thus providing a strong bond in the presence of aqueous cutting lubricants and coolants. All Aquabond thermoplastic adhesives when submerged in HOT water will go to solution and not return. The use of Aquaclean 900 and ultrasonic or air agitation greatly speeds debonding and aids in producing very clean finished parts. As long as the work piece is non- hazardous, and you already have the proper approvals, the solution can be poured down the drain.All Aquabond thermoplastic temporary adhesives come in either 100 gram bulk ingots or in 45 gram 5/8 inch diameter sticks for easy application.Aquabond 65 is a formulation with the properties of both Aquabond 55 and Aquabond 85. It is a great all purpose product for either lapping and grinding or slicing and dicing.Information provided by Aquabond Technologies.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
Solubility <= 1000 ppm
<= 1000 ppm
at 25°C
1.00e+6 ppm
1.00e+6 ppm
at 80°C
Viscosity <= 3000 cP

@Temperature 75.0 °C
<= 3000 cP

@Temperature 167 °F
Mechanical Properties Metric English Comments
Penetration <= 5.0
<= 5.0
at 25°C
Thermal Properties Metric English Comments
Melting Point 88.0 °C
190 °F
Softening Point 60.0 - 85.0 °C
140 - 185 °F
Flash Point 250 °C
482 °F
closed cup
Processing Properties Metric English Comments
Processing Temperature 50.0 - 60.0 °C
122 - 140 °F
Tacking Temperature
85.0 - 150 °C
185 - 302 °F
Bonding Temperature
Melt Temperature 85.0 - 105 °C
185 - 221 °F
Cure Time 30.0 min
0.500 hour
Cooling time
Descriptive Properties Value Comments
Color Green
Debond/Cleanup Hot DI Water and Aquaclean 900
Use of ultrasonic or injected air cleaning speeds debonding in all systems
Users viewing this material also viewed the following: