Material Notes:
Aremco-Bond 570 is a contact adhesive. Apply .015" to each part, allow solvents to flash for 20 minutes, then clamp parts together for curing.Single-Part Contact Adhesive, Excellent Flexibility
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Viscosity 35000 cP
35000 cP
Mixed Viscosity
Mechanical Properties Metric English Comments
Shear Strength 14.5 MPa
2100 psi
ASTM D1002-94
Thermal Properties Metric English Comments
CTE, linear 86.4 µm/m-°C

@Temperature 20.0 °C
48.0 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 316 °C
600 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Dielectric Strength 11.8 kV/mm
300 kV/in
Processing Properties Metric English Comments
Cure Time 48.0 min
0.800 hour
0.3 hrs at 180°F; 0.5 hrs at 350°F (Recommended Cure)
1470 min
24.5 hour
24 hrs at RT; 0.5 hrs at 350°F (Alternate Cure)
Descriptive Properties Value Comments
Chemical Resistance Excellent
Color Black