Material Notes:
Ceramic-Filled, One-Part, Thixotropic Based Paste.Used Primarily to Seal Boiler Doors and Molten Metal Systems.Easy to Apply and Removable; For uses to 2300°F
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1260 °C
2300 °F
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
1-2 hrs Air Set; 1 hr at 200°F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Gray Brwon
Filler Ceramic Fiber