Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termites.Low melt viscosity. Easy to extrude. High UV and thermal resistance.Example applications: Coating of electric and telephone cables.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Water Absorption 1.6 %
1.6 %
Melt Flow 11.3 g/10 min

@Load 2.16 kg,
Temperature 235 °C
11.3 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.0 MPa
6820 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 1.73 GPa
251 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 174 °C
345 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dissipation Factor 0.00033

@Frequency 1e+6 Hz
0.00033

@Frequency 1e+6 Hz
0.000358

@Frequency 100 Hz
0.000358

@Frequency 100 Hz