Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11 with 30% Glass Fiber Filler
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,MHL,18-050,GF30Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.Rigidity. High compressive strength. Low linear expansion coefficient. Low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability.UL classification: UL94 HB RTI(C) 65/65/65Example applications: Wind turbine, casing.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Water Absorption 1.3 %
1.3 %
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115 MPa
16700 psi
5 mm/min
Elongation at Break 7.0 %
7.0 %
5 mm/min
Tensile Modulus 8.00 GPa
1160 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Oxygen Index 22 %
22 %
Electrical Properties Metric English Comments
Dissipation Factor 0.000376

@Frequency 1e+6 Hz
0.000376

@Frequency 1e+6 Hz
0.000438

@Frequency 100 Hz
0.000438

@Frequency 100 Hz