Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11 with 10% Glass Fiber Filler
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between good impact strength and rigidity. Low linear expansion coefficient. Low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability.UL classification: UL94 HB RTI(C) 65/65/65Example applications: Sport parts.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
50 mm/min
Elongation at Break 17.3 %
17.3 %
Nominal Strain; 50 mm/min
Elongation at Yield 4.0 %
4.0 %
50 mm/min
Tensile Modulus 2.87 GPa
416 ksi
1 mm/min
Charpy Impact Unnotched 10.2 J/cm²
48.5 ft-lb/in²
10.0 J/cm²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
UL RTI, Electrical 65.0 °C
149 °F
UL RTI, Mechanical with Impact 65.0 °C
149 °F
UL RTI, Mechanical without Impact 65.0 °C
149 °F