Material Notes:
Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Very good chemical resistance.Example applications: Fuel line.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Water Absorption 1.2 %
1.2 %
Moisture Absorption at Equilibrium 0.65 %
0.65 %
Humidity Absorption
Melt Flow 4.9 g/10 min

@Load 2.16 kg,
Temperature 235 °C
4.9 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 23 %
23 %
50 mm/min
Tensile Modulus 0.555 GPa
80.5 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 0.410 J/cm²

@Temperature -30.0 °C
1.95 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C
106 °F