Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2 inch wide, 15 mil thick, pale yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Design/Construction:Interleave: 2.5 mil PolyethyleneRubber: Silicone self-fusing rubberCross-section: 2" wide rectangularThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 381 microns
15.0 mil
Rubber; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 6.55 MPa
950 psi
Silicone Property; Arlon SQA-TMS-009
Elongation at Break 425 %
425 %
Silicone Property; Arlon SQA-TMS-009
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 37.4 kV/mm
950 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Allis Chalmers Tack (inches) 0.2
Arlon SQA-TMS-013
Color Pale Yellow