Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 381 microns
15.0 mil
Nominal
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Thickness 381 microns
15.0 mil
Typical; ASTM D374
DuPont™ Nomex® N196 Paper, 15 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Thickness 381 microns
15.0 mil
Total; ASTM D3652
3M 2552/Silver Damping Foils
General purpose vibration dampingInformation provided by 3M
Thickness 381 microns
15.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 18596R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi..
Thickness 381 microns
15.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 18986XA023 0.023" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ..
Thickness 381 microns
15.0 mil
Prime Coated 1523 Fiberglass, Substrate
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
Thickness 381 microns
15.0 mil
Overall
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon 32580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s..
Thickness 381 microns
15.0 mil
Silicone; Arlon SQA-TMS-003
Arlon 32980XA015 0.015" Uncured Silicone Rubber on Polyester Film
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as ..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51586R015E 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat..
Thickness 381 microns
15.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 51866R015E 0.0150" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
Thickness 381 microns
15.0 mil
Prime Coated 1564 Fiberglass, Substrate
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, ..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-012
Arlon T4015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..
Thickness 381 microns
15.0 mil
overall; Arlon SQA-TMS-003
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon Thermabond® 99730N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub..
Thickness 381 microns
15.0 mil
Tape
3M 412DL Flexomount™ Solid Printing Tapes
3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51100R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51149R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassLayer 1: Cured Silicone RubberThis data represents typical values for the production mat..
Thickness 381 microns
15.0 mil
Overall Thickness
Arlon 51426W015 0.015" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr..
Thickness 381 microns
15.0 mil
Rubber; Arlon SQA-TMS-003
Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber
2 inch wide, 15 mil thick, pale yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part num..
Thickness 381 microns
15.0 mil
Substrate
Arlon R31030R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: 0.015" Prime Coated 1564 FiberglassThis data represents typical values for the production material and..
Thickness 381 microns
15.0 mil
Prime Coated 7628 Fiberglass, Substrate
Arlon R31961R019 0.019" (0.483 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 381 microns
15.0 mil
Liner
3M FV039 Indoor UL Recognized White Vinyl Label Products
3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,..
Thickness 381 microns
15.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 31560R015 0.015" (0.381 mm) Uncured Silicone Rubber on Release Carrier
Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE Carrier This data represents typical values for the production material. The data should not be us..
Thickness 381 microns
15.0 mil
Side 1
Arlon 44602M020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberAppearance Tan rubber on glass fiber fabricThis data represents typical values for the production material. The data should not be used to write, or ..
Thickness 381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Arlon 915-10R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and..