Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon AD250 Woven Glass and PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon AD250 Woven Glass and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0867 lb/in³
Water Absorption 0.070 %
0.070 %
Mechanical Properties Metric English Comments
Peel Strength 2.45 kN/m
14.0 pli
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C
6.67 µin/in-°F
x direction
15.0 µm/m-°C
8.33 µin/in-°F
y direction
CTE, linear, Transverse to Flow 95.0 µm/m-°C
52.8 µin/in-°F
z direction
Thermal Conductivity 0.235 W/m-K
1.63 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 1.00e+10 Hz
2.5

@Frequency 1.00e+10 Hz
2.5

@Thickness 0.381 mm
2.5

@Thickness 0.0150 in
2.5

@Thickness 3.17 mm
2.5

@Thickness 0.125 in
Dissipation Factor 0.0018

@Frequency 1.00e+10 Hz
0.0018

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -110
Copyright © lookpolymers.com All Rights Reserved