Guarniflon FEP Fluorinated Ethylene Propylene

Category Polymer , Thermoplastic , Fluoropolymer , FEP
Manufacturer Guarniflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Guarniflon FEP Fluorinated Ethylene Propylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up to 200° C. The most common format being, skived film, it can be used as non-stick material in the compression moulding processes, or melting material between fluorinated resins.Information provided by Guarniflon®
Physical Properties Metric English Comments
Density 2.14 - 2.17 g/cc
0.0773 - 0.0784 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 62
57 - 62
ASTM D2240
Tensile Strength >= 25.0 MPa
>= 3630 psi
ASTM D638
Elongation at Break >= 350 %
>= 350 %
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 80.0 - 100 µm/m-°C
44.4 - 55.6 µin/in-°F
25°C to 100°C; ASTM D696
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM D177
Melting Point 260 - 270 °C
500 - 518 °F
Electrical Properties Metric English Comments
Dielectric Strength 20.0 - 30.0 kV/mm
508 - 762 kV/in
ASTM D149