Material Notes:
Description: 1 inch wide, 50 mil thick, Red, Rectangular cross-section, Fully cured silicone interleaved with 0.002” PSA liner. Product is supplied in various roll lengths and the xx in the product number indicates roll length in yards.Design/Construction: Interleave: Mylar Pressure Sensitive Adhesive: Silicone Extrusion: Cured Silicone Rubber Cross-Section: 1” Wide RectangularArlon STD Certificate of Compliance for commercial applications will be provided with each order.Appearance: Red silicone rubber on polymer linerThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
Tape Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Interleave
1270 microns
50.0 mil
Rubber; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
Tape Property; ASTM D2240
Tensile Strength 7.557 MPa
1096 psi
Tape Property; ASTM D412
Elongation at Break 358 %
358 %
Tape Property; ASTM D412
Peel Strength 0.175 kN/m
1.00 pli
Tape Property; MIL-I-46852C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red