Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 204 °C | 400 °F | Constant |
Plasma Coatings 21000 Surface Material Information provided by Plasma Coatings |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Intermittent |
Dielectric Polymers NT-140A89 General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | continuous |
Lucas-Milhaupt Silvaloy® B72 Brazing Alloy Silvaloy B72 is the eutectic composition of the silver-copper system. It is suitable for use in controlled atmosphere brazing without the use of a paste flux. When molten, it is very fluid and may f.. |
|||
Maximum Service Temperature, Air | 204 °C @Pressure 6.89 MPa |
400 °F @Pressure 1000 psi |
Continuous |
Garlock BLUE-GARD® 3000 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fiber, high-temperature fillers, and nitrile (NBR) binder.Excellent SealabilityUnique blend of aramid fibers, fillers, and a NBR rubber binder provides improved torque retention and lowered e.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Saint-Gobain COHRlastic® CF1867 Thermally Conductive Silicone Coated Fabric Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. CF1867.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Saint-Gobain COHRlastic® F-12 Silicone Foam Description: Low-density, flame-retardant COHRlastic silicone foam yard goods provide outstanding performance for industries ranging from aviation and mass transit to automotive, electronics, constr.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Intermittent |
Saint-Gobain Versilicâ„¢ SPX-50 High Strength Silicone Tubing Formulation Description: Versilicâ„¢ SPX-50: Peroxide-cured Versilicâ„¢ High-Strength Silicone Tubing is designed for use in applications where flexibility, resiliency and durability are required. Its s.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation .. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler Description: Master Bond MasterSil 705C is an electrically conductive, one component, non-corrosive, carbon filled silicone for bonding, sealing and coating. This black colored paste like system cur.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Supreme 10HT One Component, Low Outgassing, Toughened Epoxy System Master Bond Supreme 10HT features a unique blend of performance properties including both high shear and peel strengths along with convenient handling. Supreme 10HT is room temperature storable and .. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Supreme 10HTN Nickel Filled Electrically Conductive One Part Epoxy Master Bond Polymer System Supreme 10HTN combines high shear and high peel strengths, relatively low resistance, and exceptionally easy processing. This one component (no mix) high purity nickel con.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Loctite® PST® 580 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
ConocoPhillips Tacna® Rx NLGI No. 1 Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
DuPont Teijin Films Mylar® OB13AF Polyester Film, 150 Gauge Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 51112R013 0.013" (0.330 mm) Cured, Self Fusing, Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured, Self Fusing, Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data sho.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 910-07RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 920-07Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon LW202Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Continuous |
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 915-07R##-P1 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.75” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness a.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 915-15X##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 15 mil thick, Gray, Rectangular cross-section, Self.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 920-15Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon LW201C##FR-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 20 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indica.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section:.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Intermittent |
Aremco Aremco-Bond™ 616 Electrically & Thermally Conductive Adhesive, Silver-Filled Electrically Conductive, Silver-Filled Epoxy Good Corrosion Resistance and Mechanical Strength to 360 °F Two-Part Paste |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |