Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 204 °C | 399 °F | |
Parker Chomerics CHO-LUBE 4220 Electrically Conductive Grease CHO-LUBE 4220 conductive grease is based on silicone fluid, which is characterized by unusual chemical inertness and outstanding thermal stability. It is a silver-filled lubricant designed for surfa.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Intermittent |
Dielectric Polymers NT-100A89 General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | Continuous |
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | Continuous |
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | intermittent |
Lucas-Milhaupt Silvaloy® 2M Brazing Alloy Silvaloy 2M is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | continuous |
Lucas-Milhaupt Silvaloy® A30 Brazing Alloy Silvaloy A30 does not contain cadmium and is often used as an alternate to cadmium containing alloys when the brazed assembly comes in contact with food or dairy products. Its slightly higher melt t.. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | Continuous useful temperature. |
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | Continuous useful temperature. |
Momentive Performance Materials RTV6126 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | Continuous useful temperature. |
Momentive Performance Materials RTV6196 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | continuous |
Lucas-Milhaupt Silvacore® A56T Flux Cored Brazing Alloy Silvaloy A56T Flux Cored has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on some app.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Saint-Gobain CHR® C Film Backing Silicone Adhesive Pressure Sensitive Tape Description: FEP film is used for applications requiring optical clarity, quick release, and abrasion resistance. FEP film applications include high temperature coil and capacitor wrapping, composit.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond EP21AOHT Thermally Conductive, Electrically Insulating Epoxy Master Bond Polymer Adhesive EP21AOHT is a high temperature resistant, two component, thermally conductive, electrically isolating epoxy adhesive, sealant, and coating with a forgiving 1:1 mix ratio.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Mastersil 705TC One Component, Thermally Conductive Silicone Master Bond MasterSil 705TC is a one component, thermally conductive, electrically isolating, high performance silicone for bonding, sealing and coating applications. The material is an off-white co.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Prior to fire situation |
Thermal Ceramics Min-K 1303 Data Recorder Molded Min-K Insulation Min-K Data Recorder materials (so named because of their application in protecting Flight Data Recorder and Cockpit Voice Recorder memory chips) are a specific group of materials available in two ty.. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | |
Dow Corning 7 RELEASE COMPOUND Silicone-based compound, light consistencyInformation provided by Dow Corning |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | |
Dow Corning 700 INDUSTRIAL GRADE SILICONE SEALANT General industrial sealing and adhesive applicationsInformation provided by Dow Corning |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | |
Dow Corning MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, LIGHT Phenyl-methyl silicone grease for low to high temperaturesInformation provided by Dow Corning |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | |
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 915-10R##-P2 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Certified to meet all requirements of US Military Specification A-A5.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 920-20Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon HSLW301R##-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | continuous |
Arlon Red Silicone Press Pad with Fiberglass Substrate (55393R045) Side one - cured silicone rubber, 0.014 in. (0.36 mm) minimum; Substrate - Prime Coated 162 Fiberglass, 0.018 in. (0.46 mm) nominal; Side two - cured silicone rubber, 0.013 in. (0.33 mm) minimum; 0... |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Aremco Aremco-Bond™ 631 High Performance Epoxide Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.Also available filled with aluminum oxide (Alumina) or pigments. |
|||
Maximum Service Temperature, Air | 204 °C | 399 °F | |
3M 8507 Repulpable Forms-Splicing Tape 3M™ Repulpable Forms-Splicing Tape 8507 is a specially engineered tape for forms-splicing with a thin, semi-bleached backing, a heat resistant adhesive and skip-slit for easy separation; all comple.. |