Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R3313X016-38 0.0165" (0.419 mm) Cured Silicone Rubber with Fiberglass Substrate 38" Wide  (dis

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R3313X016-38 0.0165" (0.419 mm) Cured Silicone Rubber with Fiberglass Substrate 38" Wide  (dis.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 19.0 microns
0.750 mil
Side 2
19.0 microns
0.750 mil
Side 1
381 microns
15.0 mil
1564 Fiberglass, Substrate
381 - 457 microns
15.0 - 18.0 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 25 - 35
25 - 35
Compound Property
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Elongation at Break >= 250 %
>= 250 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
Not UL recognized
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Aluminum
Total Product Weight (oz/yd2) 12.9 - 15.7
Users viewing this material also viewed the following: