Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Mylar, Interleave
178 - 229 microns
7.00 - 9.00 mil
Overall
178 - 229 microns
7.00 - 9.00 mil
Side 1
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 68
58 - 68
Compound Property
Tensile Strength >= 7.58 MPa
>= 1100 psi
Compound Property
Elongation at Break >= 200 %
>= 200 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color White
Total Product Weight (oz/yd2) 9.14 - 11.14