Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1330 Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 10.3 MPa | 1490 psi | Aluminum-Steel; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9349J Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349J epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349J is excellent for bonding many metals and woods, most plastics.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9349K Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349K epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349K is excellent for bonding many metals and woods, most plastics.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9349M Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349M epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349M is excellent for bonding many metals and woods, most plastics.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Duct 921M01 Low Viscosity Long Pot Life Silver-Filled Epoxy TRA-DUCT 921M01 is a two component, silver-filled electrically conductive epoxy adhesive designed for applications which require electrical conductivity and a long pot life at a relatively low heat .. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond 2204 Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9349 Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349 epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349 is excellent for bonding many metals and woods, most plastics a.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Grit blasted steel |
Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 10.3 MPa @Temperature 25.0 °C |
1500 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-271 Epoxy Adhesive A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled .. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP QSZ EPI Engineered Polymers Quick Set Epoxy with Zinc EP QSZ Quick Set Epoxy with Zinc, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s (Volatile Organic Compound), self-leveling modified epoxy. This versatile new gene.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea EP RAP 45 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC is, aliphatic polyurea (silicone optional) coating, that was developed for UV stable (col.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP-1567 HX EPI Engineered Polymers Aliphatic Polyurea RAP-1567 is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | cured |
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP QS EPI Engineered Polymers Quick Set Epoxy EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea f.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |