Ashley Polymers Ashlene® 527LDS Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 527LDS Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A very high impact, slightly lubricated and heat stabilized nylon resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 1.3 %
1.3 %
ASTM D570
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 10.13 J/cm
18.98 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
457 kV/in
ASTM D149