Material Notes:
Nylon 6, 30% glass reinforced resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Ultimate 131 MPa
19000 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 6.70 GPa
972 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648