Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 216 °C | 421 °F | ASTM D789 |
PolyOne Nymax™ GF 1010 14 Black 13 Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Nylene® PA6 Glass Filled 5233 HS Nylon 6 33% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Nylene® PA6 Homopolymer 201 Nylon 6; Low Viscosity Nucleated Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Melting Point | 216 °C | 421 °F | ISO 3146; ASTM D3418 |
Quadrant EPP Monocast® MC 904P Nylon for Pile Driver Pads (ASTM Product Data Sheet) Pile driver pads are used to prevent damage to the pile and the piling hammer. Fillers are usually made of hardwood - Azobe, for example. The disadvantage of Azobe is the 30-40% energy loss and it.. |
|||
Melting Point | 216 °C | 421 °F | ASTM D789 |
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melting Point | 216 °C | 421 °F | By DSC |
Toyobo PELPRENE™ S3001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melting Point | 216 °C | 421 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 216 °C | 421 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | <= 216 °C | <= 421 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at hig.. |
|||
Melting Point | 216 °C | 421 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® R 47 HW 10 PA6 Grilon R 47 HW 10 is a flexible, cold impact resistant and heat stabilized polyamide 6 for applications in the extrusion. The material can be processed on all for polyamides suitable tube-extrusion .. |
|||
Melting Point | <= 216 °C | <= 421 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi.. |
|||
Melting Point | 216 °C | 421 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |
|||
Melting Point | 216 °C | 421 °F | ASTM D789 |
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Melting Point | 216 °C | 421 °F | ASTM D789 |
Adell BJ-34 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Melting Point | 216 °C | 421 °F | ASTM D789 |
Adell BJ-37 Nylon 6, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Melting Point | 216 °C | 421 °F | ASTM D789 |
Adell BT-13 Nylon 6, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 630-13G Nylon 6, 13% Glass Reinforced A 13% glass fiber reinforced Nylon 6, designed to provide a high flexural modulus and good dimensional stability, while maintaining the ease of processing associated with Nylon 6 type materials.Data.. |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 630-33G Nylon 6, 33% Glass Reinforced Nylon 6, 33% glass reinforced resin.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 630-33GU Nylon 6, 33% Glass Reinforced Nylon 6, 33% glass reinforced resin, utility grade. Also available: 630S - 33GU Heat Stabilized, 630 - 33GBU Black, 630S - 33GBU Black with H.S.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 735LD Nylon 6 An impact modified, plasticized copolymer with improved impact resistance for injection molding.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 736LD Nylon 6 Modified to retain toughness at low temperatures for injection molding.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 827B Nylon 6 High impact, black, economy grade. Also available as: 827SB - Heat Stabilized, Black and 827SH - Heat Stabilized & UV Stabilized for Weatherability, Black.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 830 Nylon 6 Basic Nylon 6, medium viscosity, unlubricated.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 830L-30G Nylon 6, 30% Glass Reinforced A 30% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p.. |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 830LN Nylon 6 Basic Nylon 6, medium viscosity, lubricated and nucleated for injection molding.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 830LS-30G Nylon 6, 30% Glass Reinforced A 30% glass fiber reinforced Nylon 6 with heat stabilizer designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 .. |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 847 Nylon 6, Film Grade A very high impact, low flexural modulus Nylon 6 resin for molding or extrusion. Outstanding low temperature properties.Data provided by the manufacturer |
|||
Melting Point | 216 °C | 421 °F | ASTM D3418 |
Ashley Polymers Ashlene® 830L-33G Nylon 6, 33% Glass Reinforced A 33% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p.. |
|||
Melting Point | 216 °C | 421 °F | ASTM D2117 |
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang. |
|||
Melting Point | 216 °C | 421 °F | ASTM D789 |
Adell BJ-17 Nylon 6, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |