Material Notes:
A general purpose high viscosity extrusion grade Nylon 66 with very good natural color.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hrs; ASTM D570
Water Absorption at Saturation 8.5 %
8.5 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Strength 116 MPa
16800 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
ASTM D648