Material Notes:
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Physical Properties Metric English Comments
Density 1.20 - 1.24 g/cc
0.0434 - 0.0448 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 69 - 75
69 - 75
ISO 7619
Tensile Strength >= 52.0 MPa
>= 7540 psi
ISO 37
Tensile Stress >= 22.0 MPa

@Strain 100 %
>= 3190 psi

@Strain 100 %
ISO 37
>= 32.0 MPa

@Strain 300 %
>= 4640 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 350 %
>= 350 %
ISO 37
Tear Strength >= 110 kN/m
>= 628 pli
ISO 34
K Factor (Wear Factor) <= 35
<= 35
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 32 %

@Temperature 70.0 °C
<= 32 %

@Temperature 158 °F
ISO 815