Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.400 - 1.24 g/cc | 0.0145 - 0.0448 lb/in³ | Average value: 1.07 g/cc Grade Count:70 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.04 - 1.24 g/cc | 0.0376 - 0.0448 lb/in³ | Average value: 1.10 g/cc Grade Count:8 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.12 - 1.24 g/cc | 0.0405 - 0.0448 lb/in³ | Average value: 1.17 g/cc Grade Count:32 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.994 - 1.24 g/cc | 0.0359 - 0.0448 lb/in³ | Average value: 1.08 g/cc Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma.. |
|||
Density | 1.24 - 1.24 g/cc @Temperature >=250 °C |
0.0448 - 0.0448 lb/in³ @Temperature >=482 °F |
Average value: 1.24 g/cc Grade Count:1 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Density | 1.24 - 1.24 g/cc @Temperature 295 - 295 °C |
0.0448 - 0.0448 lb/in³ @Temperature 563 - 563 °F |
Average value: 1.24 g/cc Grade Count:1 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.17 - 1.24 g/cc | 0.0423 - 0.0448 lb/in³ | 262 Resin |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 64 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 70/T Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7006 Flexible PVC, Injection Molding for Footwear Soles for Cd/Pb/Ba free |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 73/T Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70/A Flexible PVC, Transparent Extrusion Transparent profiles and pipes |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 75 Flexible PVC, Transparent Extrusion Transparent profiles and pipes |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 75/UV Flexible PVC, Transparent Extrusion Transparent profiles UV resistant |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 80 Flexible PVC, Transparent Extrusion Transparent profiles and pipes |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PHA 78 Flexible PVC, Transparent Extrusion Atoxic pipes |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 264D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 272D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 298A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 464D Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 764D PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 772D PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 672D Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 0358 Flexible PVC, Insulation Transparent Cables Lead Free Transparent cables (105°C) |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 75/T Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 78/T Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 75/A Flexible PVC, Transparent Extrusion Profiles, UL 94 Class V1 |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 84/1 Flexible PVC, Sheathing Transparent Cables Lead Free Transparent cables (90°C) |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 7020 Flexible PVC, Transparent Extrusion Transparent garden hoses |
|||
Density | 1.20 - 1.24 g/cc | 0.0434 - 0.0448 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 0319/UV Flexible PVC, Extrusion Modified with PU Outdoor profiles PVC/PU anti-UV |