Material Notes:
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Physical Properties Metric English Comments
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 79 - 85
79 - 85
ISO 7619
Tensile Strength >= 30.0 MPa
>= 4350 psi
ISO 37
Tensile Stress >= 4.00 MPa

@Strain 100 %
>= 580 psi

@Strain 100 %
ISO 37
>= 8.00 MPa

@Strain 300 %
>= 1160 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 650 %
>= 650 %
ISO 37
Tear Strength >= 65.0 kN/m
>= 371 pli
ISO 34
K Factor (Wear Factor) <= 65
<= 65
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 24 %

@Temperature 70.0 °C
<= 24 %

@Temperature 158 °F
ISO 815