Axiall 1651 Clear 7002 Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 1651 Clear 7002 Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.18 - 1.22 g/cc
1.18 - 1.22 g/cc
ASTM D-792
Melt Flow 84.3 g/10 min

@Load 14.91 kg,
Temperature 175 °C
84.3 g/10 min

@Load 32.87 lb,
Temperature 347 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 69
63 - 69
delayed; ASTM D-2240
Tensile Strength, Yield 15.5 MPa
2250 psi
ASTM D-638
Elongation at Yield 410 %
410 %
ASTM D-638
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 168 °C
335 °F