Mechanical Properties Metric English Comments
100% Modulus 0.00586 GPa
0.850 ksi
STM D412
S&E Specialty Polymers TufGuard E™ XP-115DD-Zeta PE, Flame Retardant
Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers
100% Modulus 0.00586 GPa
0.850 ksi
STM D412
S&E Specialty Polymers TufGuard E™ XP-115D-Zeta PE, Flame Retardant
Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers
100% Modulus 0.00586 GPa
0.850 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00586 GPa
0.850 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00586 GPa
0.850 ksi
Shin-Etsu Silicones SFX-14036AU Fluorosilicone Elastomer
Product Description Shincor SFX14036AU is normal 75 Durometer fluorosilicone compounds. It is designed to process well in molding applications. Product Features: Excellent fuel and solvent resistanc..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D412
SK Chemicals SKYTHANE® R185A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.00586 GPa
0.850 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D638
Colorite Polymers 7284 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Axiall 7800 Moldings & Extrusions Flexible PVC
General purpose, 60°C rated molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00586 GPa
0.850 ksi
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer
AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficien..
100% Modulus 0.00586 GPa
0.850 ksi
Press Cure 10 minutes @ 177°C, Post Cure 16 hours @ 232°C
3M Dyneon™ BRE 7231 Base Resistant Elastomer
3M™ Dyneon™ Fluoroelastomer BRE 7231 is a Base Resistant Fluoroelastomer containing 60% fluorine. It is a bisphenol cured terpolymer and is categorized as a type 4 FKM per ASTM D1418. This product..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Axiall 1651 Clear 7002 Flexible PVC
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Axiall 6690 Moldings & Extrusions Flexible PVC
General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Axiall 8758 Moldings & Extrusions Flexible PVC
A general purpose extrusion compound recommended for extruded shapes, weatherstrips and flexible gaskets. Formulated for good UV light resistance and low temperature properties.Information provided..
100% Modulus 0.00586 GPa
0.850 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2120 Fluoroelastomer
3M™ Dyneon™ Flouroelastomer FC 2120 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D638
Colorite Polymers 6911X General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00586 GPa
0.850 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Axiall 18752 Wire & Cable Flexible PVC
Electrical grade extrusion compound with excellent low temperature performance. Maximum service temperature of 105°CInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20..
100% Modulus 0.00586 GPa
0.850 ksi
ASTM D-638
Axiall 83-126K Moldings & Extrusions Flexible PVC
Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.