Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 8150 Rigid PVC, Extrusion & Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8150 Rigid PVC, Extrusion & Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical ResistanceThermoformabilityExtrudability in Profile and SheetMoldability in Fittings and CapsInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 83
83
ASTM D-2240
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Tensile Modulus 2.62 GPa
380 ksi
ASTM D-638
Flexural Strength 68.9 MPa
10000 psi
ASTM D-790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D-790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
ASTM D-1822
Dart Drop Total Energy 49.1 J/cm
0.0920 ft-lb/mil
23°C, C.125 Tup, Method A; ASTM D-4226
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 66.7 °C
152 °F
annealed; ASTM D-648
Descriptive Properties Value Comments
Cell Classification 14434323
ASTM D-4216
Flow Ratio (Distance/Wall Thickness, 390-400°F) 160
Internal
Users viewing this material also viewed the following: