Material Notes:
Georgia Gulf 9017J Clear 06 is for food packaging and personal care applications requiring optimum taste and odor properties. The compound contains an ultraviolet light stabilizer, which protects light sensitive products.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Tensile Modulus 2.55 GPa
370 ksi
ASTM D-638
Flexural Strength 81.4 MPa
11800 psi
ASTM D-790
Izod Impact, Notched 1.33 J/cm

@Thickness 6.35 mm
2.50 ft-lb/in

@Thickness 0.250 in
ASTM D-256
7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 149 kJ/m²
71.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D-648
Optical Properties Metric English Comments
Haze 6.0 %

@Thickness 3.17 mm
6.0 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 77 %

@Thickness 3.17 mm
77 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 1300
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes 23